ʻO ka huahana TKYZ kahi huahana hou i hoʻomohala ʻia ma hope o ka huahana TK1, i hoʻohana nui ʻia i nā mea hoʻomehana wela uila i nā makahiki i hala. Ke hoʻohālikelike ʻia me TK1, hoʻomaikaʻi hou ʻia kona maʻemaʻe a hoʻomaikaʻi hou ʻia kona kūpaʻa oxidation. Me ka hui like ʻole o ka honua ʻokoʻa a me ke kaʻina hana metallurgical kū hoʻokahi, ua ʻike ʻia ka mea e nā mea kūʻai aku a me nā mea kūʻai aku ma ke kahua o ka wela wela a me ka wela wela. Hoʻohana maikaʻi ʻia i ka sintering ceramic, diffusion furnaces, nā kapuahi ʻoihana me ka mana kiʻekiʻe a me ka wela kiʻekiʻe.
NA ELELE KEMIIKA NUI A ME NA WAIWAI
Na waiwai \ Papa | TKYZ | ||||||||||
Cr | Al | C | Si | ||||||||
20-23 | 5.8 | ≤0.04 | ≤0.4 | ||||||||
Mahana lawelawe mau loa (ºC) | 1425 | ||||||||||
20ºC (μ.Ω.m) | 1.45 | ||||||||||
ʻO ka mānoanoa (g/cm3) | 7.1 | ||||||||||
TensileSikaika(N/mm²) | 650-800 | ||||||||||
Elongation (%) | >14 | ||||||||||
HighTemperatureSikaika(MPa) ma 1000 ℃ | 20 | ||||||||||
ola wikiwiki ma 1350 ℃ | Ma mua o80 hola | ||||||||||
ʻO kaEhoʻopaʻapaʻaOf The FullyOi hoʻopaʻa ʻiaState | 0.7 |
ʻAwelika Linear Expansion Coefficient
Ka wela ℃ | ʻAwelika hoʻonui wela × 10-6/k |
20-250 | 11 |
20-500 | 12 |
20-750 | 14 |
20-1000 | 15 |
20-1200 | - |
20-1400 | - |
ʻO ka hoʻoili wela
50 ℃ | 600 ℃ | 800 ℃ | 1000 ℃ | 1200 ℃ | 1400 ℃ | |
Wm-1k-1 | 11 | 20 | 22 | 26 | 27 | 35 |
Kū'ē wela hoʻoponopono kumu
Ka wela ℃ | 700 | 900 | 1100 | 1200 | 1300 |
Ct | 1.02 | 1.03 | 1.04 | 1.04 | 1.04 |