1. FM0 Oxford Ashloy 60Ercinu-7Tg welding rod
Ercinu-7He ikaika maikaʻi a me ke kauaʻana ma nā media lehulehu, me nā kai kai,ʻo nā paʻakai, a me ka hoʻemiʻana i nā maʻi. A hiki ke hoʻohanaʻia e uhiʻia ma luna o ka carbon cheel ʻAʻoleʻo kēia alloy he makahiki paʻakikī a i ka wā i hoʻohanaʻia e hui pū me Monel K-500 i ka ikaika haʻahaʻa ma mua o ka mea hao waihona.
Nā inoa maʻamau: Oxford alloy® 60 FM 60 teChalloy 418
Kūlana: Aws 5.4 Ernicu-7 / Asme Sfa 5.14 Tour II. 2.4377 ISo Sni4060ʻEulopa Nicu30mn3ti
ʻO ka huiʻana o ke kemika (%)
C | Si | Mn | S | P | Ni |
≤0.15 | ≤1.25 | ≤4.0 | Ç0.015 | ≤> 2.02 | 62-69 |
Al | Ti | Fe | Cu | maahua | |
≤1.25 | 1.5-3.0 | ≤2.5 | Hoʻomaha | <0.5 |
ʻO nā waihona kāwele
Ke kaʻina hana | Olemela | Lihululi | Huakai | Aila |
Tig | .035 "(0.9mm) .045 "(1.2mm) 1/16" (1.6mm) 3/32 "(2.4mm) 1/8 "(3.2mm) | 12-15 13-16 14-18 15-20 15-20 | 60-90 80-110 90-130 120-175 150-220 | 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon |
Mig | .035 "(0.9mm) .045 "(1.2mm) 1/16" (1.6mm) | 26-29 28-32 29-33 | 150-190 180-220 200-250 | 75% Argon + 25% helium 75% Argon + 25% helium 75% Argon + 25% helium |
Ikea | 3/32 "(2.4mm) 1/8" (3.2mm) 5/32 "(4.0mm) | 28-30 29-32 30-33 | 275-350 350-450 400-550 | Hiki ke hoʻohanaʻia ka flux kūpono Hiki ke hoʻohanaʻia ka flux kūpono Hiki ke hoʻohanaʻia ka flux kūpono |
Nā Pīkuhi Propertinies
Ikaika ikaika | 76,5000 psi | 530 mpa |
Ka ikaika | 52,500 psi | 360 mpa |
Ewangantion | 34% |
Noi
Hiki ke hoʻohanaʻiaʻo Erminu-7 no nā noi unahi e hoʻohana ana i nā noi Nickelila e hoʻohana ana i nā alkel-copperl-copperl
Hoʻohanaʻiaʻo Ercinu-7 no ka GAG-TUNGSTEN-Arc, Gas-Metal-Metal-Acc, a me ka ulana-arc
Hoʻohana nuiʻiaʻo Ercinu-7 i nā noi o Marine ma muli o kāna pale maikaʻi i nā hopena kūpono o nā wahi o ke kai a me nā wai brackish.