Hoʻopili:
Mea haki kaapuni haʻahaʻa voltage, relay overload thermal, uwea hoʻomehana uila, moena hoʻomehana uila, uwea hoʻoheheʻe hau a me nā moena, nā moena hoʻomehana radiant kaupaku, nā moena hoʻomehana papahele a me nā kaula, nā uwea pale hau, nā mea hōʻailona wela uila, nā uwea hoʻomehana PTFE, nā mea hoʻomehana hose, a me nā huahana uila haʻahaʻa voltage ʻē aʻe
Ka nui o nā kemika, %
| Ni | Mn | Fe | Si | Cu | ʻĒ aʻe | Kuhikuhi ROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 2 | - | - | - | Bal | - | ND | ND | ND | ND |
Nā Waiwai Mekanika
| Ka Mahana Hana Hoʻomau Loa | 200ºC |
| Ke kūpaʻa ma 20ºC | 0.05±5%ohm mm2/m |
| Ka nui o ka paʻa | 8.9 g/cm3 |
| Ka Hoʻokele Wela | <120 |
| Kiko Heheʻe | 1090ºC |
| Ikaika Tensile, N/mm2 Annealed, Palupalu | 200~310 Mpa |
| Ikaika Tensile, N/mm2 ʻōwili anu | 280~620 Mpa |
| Elongation (anneal) | 25% (min) |
| Elongation (ʻōwili anu) | 2%(min) |
| EMF vs Cu, μV/ºC (0~100ºC) | -12 |
| ʻAno Micrographic | ʻaustenite |
| Waiwai Makeneka | ʻAʻole |
Ka hoʻohana ʻana o CuNi2
Hoʻohana nui ʻia ka CuNi2 haʻahaʻa kū'ē hoʻomehana i ka mea haki kaapuni haʻahaʻa voltage, ka hoʻoili hoʻouka wela wela, a me nā huahana uila haʻahaʻa voltage ʻē aʻe. ʻO ia kekahi o nā mea nui o nā huahana uila haʻahaʻa voltage. Loaʻa i nā mea i hana ʻia e kā mākou hui nā ʻano o ke kūpaʻa kū'ē maikaʻi a me ke kūpaʻa kiʻekiʻe. Hiki iā mākou ke hoʻolako i nā ʻano uea poepoe, pālahalaha a me nā mea pepa.