Nickel alloy monel k-500, a me nā makahiki he nui, a me ka loaʻaʻana o ka manikini maikaʻi loa, a me nā loaʻaʻana o ka ikaika loa a me ka mālamaʻana i kona ikaika
ʻO ka paleʻana o ka corrosioni o Monel K-500 i like me ka moʻama 400 wale nō, ma keʻano he nui o keʻano.
ʻO kekahi o nā noi maʻamau o Nickel Alaman K-500 no nā kīwaha kīwī, nā mea hana olakino, nāʻano uila me nā uila uila. Hoʻohana muaʻia kēia alloy i ka marine a me nā lako hana a me nā lako hana. Ma ka hoʻohālikelikeʻana o ka molnel 400 iʻoi aku ka nui o ka hoʻohanaʻana i nā hale noho, nā hana likeʻole, a me nā hana likeʻole a me nāʻoihana penetochemical mau mea nui, a me nā mea'ē aʻe he nui.
Kinohi
Kumu | Ti% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
Molnel k500 | Min 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Max 2.0 | Max 1.5 | Ma ka 0,81 | Max 0.25 | Max 0.5 |
Nā kiko'ī
ʻAno | Kū-starder |
Molnel k-500 | UNT N05500 |
Bar | Astm b865 |
Nā hāmeʻa | AMS4676 |
Nā pepa hele / papa | Astm b865 |
Kākau | Awa b564 |
Nā Weld | Ercinu-7 |
Nā Pūnaewele Pūnaewele(20 ° C)
Kumu | Huakai | Malting Point | ʻO keʻano o ka uila | ʻO keʻano o ka hoʻopiʻiʻana i ka hoʻonuiʻana | Ka HōʻaʻO Kokua | Wela wela |
Molnel k500 | 8.55g / cm3 | 1315 ° C-1350 ° C | 0.615 μ • m | 13.7 (100 ° C) A / 10-6 ° C-1 | 19.4 (100 ° C) λ / (w / m • ° C) | 418 j / kg • ° C |
Nā Pīkuhi Propertinies(20 ° C min)
Molnel k-500 | Ikaika ikaika | Hāʻawi i ka ikaika RP0.2% | Ellingation A5% |
Anneed & Aged | Min. 896 mPA KAKAHI | Min. 586MPA | 30-20 |