NICHIME-60 CRATING (NICR0 TYP60 Typ0 ALLY 675 NICKEL CHROME MRROMO)
Nickel: 57-58%, Chromium: 16%, Silika: 1.5%,ʻona
Ua hana mākou he 50, 16-22, 24, 25, 28, 29 a me 31 a me 31 mau kapa i kūʻaiʻia e ka wāwae (ka mea hoʻohana maʻamau. Pono paha e koi i kahi hoʻokolohua e hoʻoholo ai i ka gauge maikaʻi loa e hoʻohana ai no kāu mea, a he aha keʻano kūpono a me keʻano kūpono.
ʻO nā waiwai o Nokr 60 Type 675 alloy:
Density (kaumaha i kēlā me kēia cubic inch:) 0.2979 lbs.
Scivity gravisty @ 68 ° F (20 ° C): 8.247
Magnetic Wittraina: Para
Watmom of themmallis Watts / cm / ° c @ 100 ° C (212 ° F): 0.132
Match apple Melting point: 2462 ° F (1350 ° C)
ʻO ka papa hana nui: 1652 ° F (900 ° C)
Nā kumu pale:
ʻO ka mahana 68 ° F (20 ° C), Factor 1.000
Mahana 212 ° F (100 ° C), factor 1.019
Mahana 392 ° F (200 ° C), factor 1.043
ʻO ka lā 572 ° F (300 ° C), factor 1.065
Mahana 752 ° F (400 ° C), factor 1.085
Ma ke kauwela 932 ° F (500 ° C), factor 1.093
Mahana 1112 ° F (600 ° C), Factor 1.110
Mahana 1292 ° F (700 ° C), factor 1.114
Ka wela 1472 ° F (800 ° C), factor 1.123
Ke kauwela 1652 ° F (900 ° C), factor 1.132
EXPE MAX DEPERS EXPY EXPY: Kaohiʻana o ka 20ºC: Kaumaha: Ka Ho'ōla O ke Kani: ʻO ka maikaʻi o ka hoʻonui nuiʻana o ka Melting point: E halawai: Nā Kūlana Microophichic: Ignetic waiwai: | 1150ºcccc 1.12 ohm mm2 / m 8.2 g / cm3 45.2 KJ / m · pua 17 × 10-6 / (2020 ~ 1000ºC) He 130ºC Min 20% Austente nonmagnetic |